Montell Adflex KS-084P TPO Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Extrusion Key Features: high melt flow, low modulus, impact resistant thermoplastic olefin, resin, good heat sealability, outstanding puncture resistance, excellent balance of flexibility, excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable Applications: extrusion coatings on a variety of substrates, film, fiber Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600. Description: Adflex KS-084P high melt flow, low modulus thermoplastic olefin resin is designed for many commercial and industrial extrusion applications. It is based on material produced from Montell's proprietary Catalloy process. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|