Montell Adflex KS-221P TPO Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Injection Molding/Impact Modification Key Features: low modulus, impact resistant thermoplastic olefin resin, flexible feel, excellent cold impact resistance, excellent stiffness and impact balance, colorable and paintable, FDA acceptable Applications: closures, lid stock, air bag door covers, impact modification Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600. Description: Adflex KS-221P low modulus thermoplastic olefin resin is designed for impact modification and injecting molding applications. It is based on material produced from Montell's proprietary Catalloy process, exhibiting balanced strength, toughness, and flexibility. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Tear Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|