Montell Adflex Q 302 B TPO Resin

 

Subcategory: Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:

Key Features: anti-gas fading, thermoplastic olefin resin for soft touch blow molding, FDA acceptable, soft touch, velvety texture, excellent strength and puncture resistance, squeezable, high heat performance, excellent chemical and environmental stress-cracking resistance, recyclable with polyethylene and polypropylene bottles, regrind maintains soft feel

Applications: blow molded bottles, squeezable containers, toys

Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.

Description: Adflex Q 302 B thermoplastic olefin resin is an innovative new packaging material that resists gas fading and brings a warm and sensual feel, creating a truly unique sensation. Part of a family of polymer with a soft, velvety texture, this resin enables packagers to give their products a distinct edge over conventional plastics. Bottles blow molded from this resin convey and upscale, quality image that enhances point of purchase appeal. The unique texture is also ideal for applications requiring a no-slip surface, such as shower soaps and lotions. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。