Montell Adsyl 5C30F Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Film extrusion Key Features: thermoplastic olefin resins for film extrusion, good clarity and gloss, good moisture barrier properties, very low seal initiation temperature, FDA acceptable Applications: food and non-food packaging, lamination films Meets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications. Description: Adsyl 5C30F thermoplastic olefin resin are designed for film extrusion applications. It is a barefoot formulation. This resin is based on materials produced by Montell's proprietary Catalloy process. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|