Montell Astryn 65F4-4 Polypropylene Homopolymer, 40% Talc
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, high stiffness, good dimensional stability, excellent heat resistance Applications: automotive heater and A/C housings, small and large appliances, fan shrouds, housewares, utility products Description: Astryn 65F4-4 conventional melt flow, 40% talc-filled polypropylene homopolymer is designed for maximum stiffness, good dimensional stability and excellent heat aging performance. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|