Montell Astryn 68F4-2 Polypropylene Homopolymer, 20% Talc
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: fractional melt flow, medium high modulus, mineral-filled, blow molding and extrusion grade polypropylene homopolymer, excellent impact and stiffness balance, good processability Applications: automotive under-the-hood components Description: Astryn 68F4-2 fraction melt flow, 20% talc-filled, blow molding and extrusion grade polypropylene homopolymer is designed for high strength, stiffness, impact resistance and processability. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|