Montell Astryn 7523C Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: conventional melt flow, medium modulus polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, versatile, good processability Applications: automotive hush panels, kick plates, stowage bins Description: Astryn 7523C conventional melt flow, precolored polypropylene copolymer has a good balance of impact resistance, flexibility and processability. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|