Montell Astryn BB77G Polypropylene Copolymer, 15% Talc
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, good impact stiffness and balance, good dimensional stability, good colorability, good aesthetics, excellent processability, good weatherability Applications: automotive interior trim components, pillar moldings, sail panels Description: Astryn BB77G high melt flow, UV-stabilized, 15% talc-filled polypropylene copolymer has an excellent balance of properties, Designed for automotive interior trim applications, this material colors easily, processes very well and provides parts with outstanding surface appearance. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact Resistance
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|