Montell Astryn BR33GC Polypropylene Copolymer, Mineral Filled
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: conventional melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, high rigidity, high impact strength, good dimensional stability, low fogging Applications: knee bolsters, map pocket bins, glove box doors Description: Astryn BR33GC conventional melt flow, UV-stabilized, precolored, mineral-filled polypropylene copolymer has an excellent balance of rigidity, impact strength and dimensional stability. It was designed for a variety of automotive interior trim applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact Resistance
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|