Montell Hifax CA187 Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balance Applications: painted automotive bumper fascias Description: Hifax CA187 medium melt flow, paintable thermoplastic elastomeric olefin resin has an excellent combination of processability and painability. It was designed primarily for painted automotive bumper fascia applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|