Montell Hifax CA199AC Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: low melt flow, medium low modulus, paintable thermoplastic olefin resin, excellent balance of properties, high toughness, good paintability, flexible Applications: automotive air bag door covers, closures and lid stock Description: Hifax CA199AC low melt flow, paintable thermoplastic olein resin exhibits balanced strength, thoughness, flexibility and ductility. It is based on material produced from proprietary Montell process technology. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Low Temperature Gardner Impact
- Impact Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|