Montell Hifax CA45 Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, excellent balance of properties, excellent processability, good colorability, excellent surface appearance Applications: molded-in color automotive bumper fascias and step pads, air deflectors, appliques Description: Hifax CA45 medum melt flow, reactor grade thermoplastic elastomeric olefin resin has a very good balance of properties and excellent moldability. It was designed primarily for molded-in color automotive exterior components and is based on material from Montell's Spheripol process. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|