Montell Hifax ETA-3081 Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good surface appearance Applications: molded-in color and painted automotive bumper fascias, air deflectors, step pads and filler panels, license plate pockets Description: Hifax ETA-3081 medium high melt flow, paintable thermoplastic olefin resin has a vry good combinatio of physical properties, modability and paintability. An extemely verastile material, it was desgined for a wide variety of apinted and modled-in color automotive exterior components. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Low Temperature Gardner Impact
- Impact Test
- Tear Strength
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|