Montell Hifax ETA-3104HF Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processability Applications: molded-in color automotive bumper step pads, rub strips, sight shields, scuff plates Description: Hifax ETA-3104HF, medium melt flow, thermoplastic elastomeric olefin resin has a very good combination of properties and prcessability. It was designed for a varity of molded-in color automotive exterior components and is available in UV-stabilized form for that purpose. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched, Low Temp
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|