Montell Hifax ETA-4161UV Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: fractional melt flow, medium high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good melt strength, excellent weatherability, excellent processability Applications: thermoformed sheet Description: Hifax ETA-4161UV fractional melt flow, UV-stabilized, extrusion grade thermoplastic olefin resin has an excellent combination of stiffness, impact resistane, melt strength, weatherability and processability. It was designed to accommodate specific thermoformed applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Tear Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|