Montell Hifax TRA-3263EC/1 Thermoplastic Olefin Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: fractional melt flow, high modulus, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good surface appearance, excellent processability Applications: extruded profiles, luggage rack inserts Description: Hifax RTA-3263EC/1 fractional melt flow, mineral-filled, extrusion grade thermoplastic olefin resin has an excellent balance of stiffness, impact strength and processability. It was designed primarliy for extruded automotive exterior applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Low Temperature Gardner Impact
- Tear Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|