Montell Hivalloy G7055 Engineering Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: glass reinforced engineering resin for injection molding, provides excellent toughness, good stiffness and strength Applications: industrial striking tools Description: Hivalloy G7055 is am impact modifed glass reinforced resin which provides oustanding toughness, as well as stiffness and strength, for a variety of industrial and comsumer applications. Material is used for applications where stiffness and low temperature impact are needed. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Processing Temperature
- Middle Barrel Temperature
- Nozzle Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|