Montell Hivalloy W011MR Engineering Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: general purpose engineering resin for injection molding, high or low gloss, good weathering characteristics, good chemical resistance, good scratch and mar performance Applications: industrial and consumer applications Description: Hivalloy W011MR is designed for both high gloss or low gloss moldedin color exterior trim for outstanding automotive, industrial, or consumer applications. The product provides oustanding weathering characteristics, chemcial resistance, and scratch and mar performance. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Middle Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|