Montell Refax RE 65F4-4 Recycled Polypropylene, 40% Talc
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: 25% post-consumer, 40% talc filled polypropylene homopolymer resin Applications: automotive, appliance, housewares Description: Refax RE 65F4-4 40% calcium carbonate-filled polypropylene copolymer resin is a compounded product containing 25% post-consumer recycled polypropylene and 75% Montell homopolymer resin. It is designed for injection molding applications. This resin is available in natural color and black. It is not intended for food contact applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|