Montell Polybutene-1 PB 0800
Subcategory: Polybutene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptable Applications: concrete carrier Meets FDA requirements in 21 CFR 175.105 for indirect food contact. Description: Polybutene-1 PB 0800 is a highly isotactic, seim-crystalline homopolymer which can be used where creep resistnace, environmental stress crack resistance and elevated temperature performance are key requirements. This polymer is miscible with polypropylenes due to its similar molecular structure. In bends with polyethylenes it is immiscible but easily dispersible. It is mainly used as a concentrate carrier and in hot adhesives where service temperatures, high strength and/or long open time are required. This copolymer meets FDA requirements for direct food contact under regulation 21 CFR 177.1570. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|