Basell Adflex™ KS089P Polyolefin
Subcategory: Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Adflex™ KS089P thermoplastic olefin resin with slip and antiblock, is designed for air quenched blown film applications. Adflex™KS089P resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for rubber articles for repeated use. The final item is subject to the extraction requirements in 21 CFR 177.2600. All ingredients meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: film Information provided by Basell.
| Available Properties |
- Density
- Water Vapor Transmission
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Coefficient of Friction, Static
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|