Basell Adflex™ Q 200 F Polyolefin
Subcategory: Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Adflex™ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's proprietary "Catalloy" process. This resin is ideal for making soft hygienic or heavy duty films. It can also be used to modify LDPE or LLDPE resins in order to improve mechanical characteristics, puncture resistance and to allow further downgauging. It contains no slip or antiblock. Q 200 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, except for certain fatty foods. Uses: Film, automotive applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|