Basell Adflex™ Q 301 F Polyolefin
Subcategory: Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Adflex™ Q 301 F thermoplastic olefin resin is designed for impact modification of polypropylene, as well as monolayer and multilayer air quenched blown films (no slip, no antiblock). It is based on proprietary Basell process technology. This resin has no slip or antiblock and only minimal stabilization in order to allow wider design latitude for the compounder. Additional suitable stabilization is recommended to protect the resin during melt processing and throughout its useful life. Adflex™ Q 301 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, except for certain fatty foods. Uses: Film, multilayer film, lawn and garden equipment, toys Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|