Basell Adflex™ Z104S Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Adflex™ Z104S, a versatile thermoplastic olefin resin, can be used for injection molding, impact modification, extrusion coating or film and fiber applications. This resin is based on proprietary Basell technology and can be used on conventional injection molding or extrusion equipment. Z104S resin features a very high softness and low modulus, with a high melt flow. It is ideal for the modification of polypropylene without altering the transparency of the modified polypropylene (homopolymer or random copolymer). It meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. The final item is subject to the extraction tests specified in 21 CFR 177.2600. All ingredients in Z 104 S resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Household goods, toys Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|