Basell Adsyl™ 3 C 37 F HP Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Adsyl™ 3 C 37 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. It contains anti-blocking and slip agents. Adsyl™ 3 C 37 F HP features a Seal-Initiation Temperature (SIT) of 112°C measured on bi-oriented film of 30 µm. With a Melting Point at 140°C, this grade exhibits an exceptionally broad processability range of temperature. The composition of the product complies with FDA norms and with regulations in force in major European concerning food contact applications. Uses: bi-oriented film Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Heat Seal Strength Initiation Temperarture
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|