Basell Hifax™ CA1110/2AC Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: Hifax™ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact resistance and paintability. It was designed primarily for use in painted automotive bumper fascia applications. Uses: Automotive exterior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Multi-axial Impact @ -30°C Total Energy
- CTE, linear 100°C
- Shrinkage
|
|
|
|
| Property Data |