Basell Hifax™ CA207A Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: Hifax™ CA207A thermoplastic olefin resin is designed to reduce shrinkage and improve paint adhesion of PP compound. It is based on proprietary Basell process technology. All ingredients in "Hifax" CA207A resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Compounding Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|