Basell Hifax™ CA287 Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: Hifax ™ CA287 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: - Good Stiffness
- Good Processability
- Good Impact Resistance
- Good Colorability
- Paintable
- Medium Flow
Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Dart Drop, Total Energy
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|