Basell Hifax™ CB247G Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hifax™ CB247G high melt flow, 1,700 MPa flexural modulus, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of properties and processability. It was designed for selected automotive interior and exterior components. Uses: Automotive applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Dart Drop, Total Energy
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|