Basell Hifax™ CB252 Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hifax™ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidity, impact resistance and paintability. It was designed primarily for automotive exterior ornamentation applications, but also has utility in certain interior trim components requiring high impact resistance. Uses: Automotive exterior and interior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Dart Drop, Total Energy
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|