Basell Hifax™ HSBMCB1158LS Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impact resistance, dimensional stability and paintability. It was designed for thin-walled bumper fascia applications that require high paint durability. Features include: high flow, high stiffness, excellent impact resistance, good mold filling capability, good dimensional stability, and very good paint durability. Typical applications include painted automotive thin-walled bumper fascias. Uses: Fascias Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|