Basell Hifax™ RTA3263/2 Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hifax™ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impact strength and paintability. It was designed primarily for rigid automotive exterior ornamentation applications. Uses: Automotive exterior parts Information provided by Basell.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Dart Drop, Total Energy
- Tear Strength
- Gardner Impact @ -30°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|