Basell Hifax™ RTA3263EUV Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hifax™ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, impact resistance, melt strength, processability and weatherability. It was designed specifically for thermoformed applications. Uses: Sheet Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Dart Drop, Total Energy
- Tear Strength
- Gardner Impact @ -30°C
- Izod Impact, Notched
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|