Basell Hostacom™ 62F4-2C Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ 62F4-2C high melt flow, 1,900 MPa flexural modulus, precolored, 20% talc-filled polypropylene homopolymer has excellent heat aging characteristics, high chemical resistance and easy processability. Uses: Appliances, automotive applications, electrical parts, household goods Information provided by Basell.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |