Basell Hostacom™ 6551 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Hostacom™ 6551 conventional melt flow, 1,300 MPa flexural modulus, precolored polypropylene homopolymer has a good combination of strength, stiffness, impact and heat resistance. It was designed for a variety of industrial and consumer applications. Uses: Electrical parts, appliances, industrial applications, consumer applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|