Basell Hostacom™ AE716BC Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ AE716BC conventional melt flow, 1,400 MPa flexural modulus, UV-stabilized, 40% calcium carbonate-filled polypropylene homopolymer has a good balance of properties and processing. It was designed to meet UL 746B (F1) requirements for outdoor applications. Uses: Electrical parts, outdoor applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|