Basell Hostacom™ BC142/1AC Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It was designed primarily for structural automotive interior components that require high rigidity and low odor. Uses: Automotive interior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|