Basell Hostacom™ BG722AC Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ BG722AC medium high melt flow, 1,700 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer is designed with an excellent balance of stiffness, impact resistance and processability. Uses: Automotive interior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Shrinkage
|
|
|
|
| Property Data |