Basell Hostacom™ BG749GC/1 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination of stiffness and processability. It was designed primarily for applications that undergo extended outdoor exposure. Uses: Outdoor applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
|
|
|
|
| Property Data |