Basell Hostacom™ BG751P Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ BG751P very high melt flow, 1,600 MPa flexural modulus, UV-stabilized, natural, 20% calcium carbonate-filled, modified polypropylene resin has a unique balance of processability and weatherability. It was designed for applications that undergo extended outdoor exposure. Features include: superior moldfilling capability, excellent weatherability, good impact/stiffness balance, and excellent surface appearance. Typical applications include residential siding panels. Uses: Outdoor applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- CTE, linear 100°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|