Basell Hostacom™ CA270G Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: Hostacom™ CA270G fractional melt flow, 140 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of grain retention characteristics, soft feel, environ-mental aging performance and low temperature ductility. It was designed primarily for thermoformed and low-pressure injection molded (LPIM) automotive instrument panel and door panel skins. Uses: Automotive interior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Compression Set
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|