Basell Hostacom™ CB275FC Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ CB275FC high melt flow, 1,900 MPa flexural modulus, precolored, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity and impact and scratch and mar resistance. It was designed for automotive interior components that must have a very good impact/stiffness balance such as instrument panels or other componentry that require compliance to FMVSS201 or FMVSS208. Uses: Automotive interior parts Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|