Basell Hostacom™ TRC704D Thermoplastic Polyolefin Elastomer
Subcategory: Elastomer, TPE; Polyolefin; Thermoplastic
Material Notes: Description: Hostacom™ TRC704D medium high melt flow, 1,500 MPa flexural modulus, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and processability. It was designed for applications that require excellent aesthetics and a good balance of stiffness and impact performance. Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|