Material Notes: Description: Hostacom™ TSOP-UM5 high melt flow, 2,000 MPa flexural modulus, natural, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of properties and processability. It was designed for a wide variety of automotive interior trim components. Features include: high rigidity, excellent moldfilling capability, excellent impact/stiffness balance, and excellent part aesthetics. Typical applications include: automotive interior trim components, door panels, instrument panels, and pillar moldings. Uses: Automotive interior trim, automotive instrument panel Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- CTE, linear 100°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|