Basell Hostacom™ ZG750 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: Hostacom™ ZG750 conventional melt flow, 1,700 MPa flexural modulus, 40% calcium carbonate-filled, utility grade polypropylene copolymer resin has a very good combination of strength, stiffness and impact resistance. Features include good impact/stiffness balance and good processability. Uses: Industrial applications Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Dart Drop, Total Energy
|
|
|
|