Basell Metocene X50109 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Metocene X50109 resin is a nucleated metallocene-catalyzed polymer for thinwall injection molding. Metocene X50109 resin meets FDA requirements in the code of Federal Regulations, 21 CFR 177.1520, for food contact, including cooking applications. All ingredients in Metocene X50109 meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Thin-walled parts, labware, household goods, closures, transparent or translucent parts, media packaging Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|