Basell Metocene X70293 Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Metocene X70293 is a metallocene-catalyzed polymer for thin wall injection molding. It is nucleated and contains an antistat. Metocene X70293 resin meets FDA requirements in the code of Federal Regulations, 21 CFR 177.1520, for food contact, including cooking applications. All ingredients in X70293 meet the chemical registration of TSCA (U.S.) and DSL (Canada). Uses: Thin-walled parts, lids, labware, household goods, cups, closures, media packaging Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|