Basell Moplen HP400H Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications of Moplen HP400H are thermoformed tubs and containers, medium draw trays and blister packs, flowerpots and small extrusion blow molded bottles. Moplen HP400H is suitable for food contact. Uses: Thermoformed containers, bottles Information provided by Basell.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Ball Indentation Hardness
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|