Basell Moplen HP400L Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure caps Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|