Basell Pro-fax™ 8301S Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Description: Pro-fax™ 8301S reactor grade polypropylene impact copolymer resin is available in spherical particle form. Spherical form resin is well suited for mixing with pigments and other additives to make polymer concentrates or masterbatches. This resin has very minimal stabilization, which allows wide design latitude for the compounder. Additional suitable stabilization is required to protect the resin during melt processing and throughout its useful life. All ingredients in Pro-fax™ 8301S resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Compounding Information provided by Basell.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|